Full Record Display for the EPA National Library Catalog

RECORD NUMBER: 77 OF 102

Main Title Reclaiming Fiber from Newsprint Dry Methods.
Author Gunderson, D. E. ; Scott, C. T. ; Geisner, R. L. ; Harten., T. M. ;
CORP Author Environmental Protection Agency, Cincinnati, OH. Risk Reduction Engineering Lab. ;Forest Products Lab., Madison, WI.
Publisher c1992
Year Published 1992
Report Number EPA/600/J-92/102;
Stock Number PB92-153949
Additional Subjects Newsprint ; Waste papers ; Waste recycling ; Fibers ; Paper industry ; Dry methods ; Dewatering ; Moisture content ; Feasibility studies ; Materials recovery ; Design criteria ; Waste management ; Pulping ; Paper products ; Reprints ; Deinking
Holdings
Library Call Number Additional Info Location Last
Modified
Checkout
Status
NTIS  PB92-153949 Some EPA libraries have a fiche copy filed under the call number shown. 07/26/2022
Collation 17p
Abstract In the study the authors examine the fiber preparation processes with the objective of demonstrating that dry-disintegration is feasible and capable of yielding a useful fiber. The project is linked with research directed toward dry and semi-dry forming methods. The fiber product is rated on the basis of yield, fiber length, and the formation, strength, brightness and opacity of a paper specimen formed by standard wet-process methods. At 18% moisture content, crumbs of dewatered pulp have been processed in disk refiner to yield fibers suitable for air forming. In the 'best effort to date' fiber length (weighted) was 1.20 mm, not significantly different from the wet-slushed control at 1.26 mm. Other methods and moisture values yielded lengths as short as 0.88 mm. Tensile index and tear for handsheets from the furnished were 16.2 Nm/g and 139 mN; well below 27.0 Nm/g and 273 mN for the control. Press drying doubles the performance of the wetlaid sheets, however, causing even the dry fiberized furnish to approach virgin newsprint strengths. Performance of early air-formed sheets was 50-60% that of water-laid, press-dried sheets. Results to date show that dewatered crumbs of ONP can be fiberized with good yield at moisture contents in the range from 6% to nearly 60%. Damage to the fiber is greatest at lower moisture content and decreases as moisture level is elevated.
Supplementary Notes Pub. in Jnl. of Hazardous Materials, v29 n2 p297-311 Jan 92. Prepared in cooperation with Forest Products Lab., Madison, WI.
NTIS Title Notes Journal article.
Title Annotations Reprint: Reclaiming Fiber from Newsprint Dry Methods.
Category Codes 68C; 71R
NTIS Prices PC A03/MF A01
Primary Description 600/14
Document Type NT
Cataloging Source NTIS/MT
Control Number 212823373
Origin NTIS
Type CAT